    There are several electronic "gold analyzer" gadgets. They have
    serious limitations like the surface quality affecting accuracy. Be
    careful, do not overestimate the accuracy-real fire assays are very
    inexpensive these days. Often less than $25.00 

    My opinion is that the most accurate small machines can be off a
    karat or two. Even XRF (relatively large expensive electric machines)
    can be inaccurate with poor samples or methods. 

    The best one I have used is the GXL-24PRO from TRI-ELECTRONICS
    patent 4799999 

    Their phone (on my old machine the area code may have changed) Fax
    619-571-5404 

    Phone 800-445-4241 

    Tri Electronics 800-445-4241 

    I use this machine regularly. I admit I still prefer my old
    fashioned scratch stone and a variety of acids for gold, silver and
    platinum. Given both methods I get fooled very very rarely, after all
    I work at a gold refinery where we spot check incoming goods. I sure
    like it when I can return a non-gold item intact to the customer
    rather than asking then to accept our opinion on faith alone.... 

Daniel Ballard
Precious Metals West


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project