Dear Jeffrey,

    The information supplied by Eddie Bell is very good and here are a
    few more comments. 

    At area of contact between rolls and material, the rolls flatten and
    forms a flat along the roll. On leaving, the rolled product returns
    elastically to their radius. 

    The smaller the diameter of the roll, the faster the curve of the
    roll falls away from the product and a smaller width of flat is made
    - thus leaving more of the available torque to flatten the product
    rather than deform the rolls surface. In other words, more of the
    rolls separating force can be used to thin the product. 

    As a rough formula an idea of the thinnest thickness can be found by
    dividing the roll diameter by a factor 700. This factor is only a
    guide and can vary from 600 - 1000 depending on product material,
    it's hardness, roll quality and rigidity of machine. Also, adding
    tension to the product at entry or exit of the rolls (or both)
    assists in making a thinner product as does frequent annealing. 

Matthew Durston
Durston Rolling Mills
www.durston.com


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project