    Hi, I have been using alum for years and have never had any poblems
    with disposal or fumes. It is relatively clean (used as a floculant
    for cleansing water). As long as you use a pickle unit or slow
    cooker (cheaper to buy) and keep the unit warm, oxides are removed
    effectively without acids. Alum should be avaliable through a
    pharmacy or drug store as the say in the US. 

    P.S you can also grow some really cool crystals. Oh by the way I
    dilute 3 parts water for 1 part Alum approx. But if you need a
    stronger solution add more Alum. Time to change? When solution
    appears blue. Probably saturated with copper and thus no longer
    effective. Time for a new solution. I am not sure on the disposal
    protocols in your country but I would imagine it would be very low
    level waste. probably equaliviant to grey water. 

Best regards
Terence M Dillon



____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project