	1.  Obtain Alum at the grocery store.

	2.  Dissolve in water obtained from your tap. 

	3.  Heat it up, and try it.

	4.  If it's too slow for you, add more alum.

    	5.  It's saturated if, upon cooling, some crystallizes back out,
    and then you know it's as strong as it can get.  If you need faster
    pickle than it will be at this point, go back to sodium bisulphate. 

    Geez.  Do we really need a recipe for this? 

    sorry.  Not to be rude or anything.  But what ever happened to just
    trying something without being afraid of screwing it up?  I can see
    wanting instructions for complex things.  But pickle?  Am I missing
    something here? After all.  We're talking about mixing two food grade
    materials here.  one is alum, an additive in pickling, and therefore
    essentially edible, in small quantities, and water, which is
    hopefully also drinkable in your location... 

Peter


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project