    Perhaps some of the readers familiar with enameling could share
    their wisdom on Johnson Matthey's Blythe Enamels. 

    Just how acid and chemical resistant are the older transparent
    Blythe enamels? 

    In particular, # 225 Green (date on package is 9 December 1975) & #
    788 Blue (not dated on package ...may be mid 1970's too). My
    original 1/2 kilo packages for #'s 225, 788 & 2092 indicate
    transparent colors. 

    In Jeanne Werge-Hartley's book she provided a very useful table of
    technical information on firing temperatures (attributed to Vitrum
    Signum on pg. 162). However, I have an information void when it
    comes to chemical and acid resistance of these transparents; and I
    am contemplating electroforming some Blythe enameled pieces. 

    As I recall; the following are probably 25 year old Blythe product.
    Possibly someone knows of an old Blythe product profile similar to
    that found in "Enameling on Precious Metals" with technical data on
    temps and flow point for the following (not found in Jeanne's book): 

	OPAQUES 
	557     Purple
	682     Green
	684     Blue
	1924    Blue
	2174    Blue
	3016    Brunswick Green K31
	3040    Mauve A25
    
	Transparent 
	225     Green       (date on package is 9 December 1975)
	242     Chedron
	788     Blue        (not dated on package may be mid 1970's)
	935     Red
	1072    Yellow
	2092    Gray Green  (date on package is 5 Aug 1978)
    
	Opalescent  
	1533    White

Regards,
Mark


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project