========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Warren: Sounds like you have a metal contamination or some other alloy problem. The only thing I can think of that will make the metal crumble. I suggest you start with a new batch of silver and use a rolling alloy until you get the hang of it and then try mixing your used scrap 50/ 50 with fresh metal.. Give a call to one of the refining houses and tell them what you need in an alloy and see what they recommend. I personally use United Precious Metals S88 master alloy for sterling, which is a low ox alloy. I use it for casting as well as milling and have had no problems. I have however found that it does work harden a little faster that milling stock and has to be annealed more frequently when hammer forging. Frank Goss ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project