    Ok I have to chime in on this one because casting precious metals
    has been the story of my miserable life for the last 15 years. What
    you really have to look at is the location and shape of the gate on
    your piece. I see pieces gated for every reason under the sun EXCEPT
    for the purpose of getting a good casting. We gate for ease of
    cleaning, we gate for ease of mold cutting, we gate to make it look
    nice ( the gate that is, I'm not kidding). The last thing on anyone's
    mind is getting a solid casting. Make the gates round!!!  Don't pinch
    the ends!!!  Fillet the joints!!! Gate to the thickest part of the
    Piece!!! Use multiple gates if you have to. Better to make a good
    casting that hard to finish then a bad casting that's easy to finish.
     I've been fighting this mind set for years. Do all the above and you
    can cast with the mold at room temperature and get fill. I've done
    it.  Hey, there's a reason why the water pipes in our houses are
    round and not square or flat!  Ok, off the soap box. 

Tino Volpe
Metallurgist, Technical Manager
Tiffany & Co.
300 Maple Ridge Drive
Cumberland, RI 02864-8707
401-288-0124


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project