The Gem and Jewelry World's foremost Resource on The Internet.
[Orchid] Rolling Sterling Ingots  
  [Thread Prev] [Message Prev]      [Date Index]   [Thread Index]      [Message Next] [Thread Next]
From: Warren
Date: Sun Nov 02 22:12:52 2003
 
     
========[ Invite a Friend - http://www.ganoksin.com/invite.htm  ]========


    Hi All, Somewhat related to my previous post about rolling mills, I
    am going to purchase one primarily to be able to create some stock a
    little heavier than the 10ga I can easily get. In the past my
    attempts to recycle scrap sterling met with disaster-crumbly pitted
    ingots the norm. I was using "clean scrap" ie no solder but it had
    been heated. I don't recall how I cleaned it but I was using a high
    quality flux in the melting of it. I mastered getting a nice pour
    with no folds but even annealling after every pass through the mill
    gave me the same resluts. 

    This time I'm determined to get it right even if I have to use
    casting grain. I'm not interested in recycling as much as the
    finished product. Would fresh casting grain be a solution? Any secret
    fluxes or crucibles? ingot molds? I was using the 2 piece molds
    getting 3"x5/8" ingots but tried th longer oepn molds with worse
    results. 

    Any ideas would be great. Thanks, Warren Allen 



____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project