From: warren allen
Date: Sat Nov 01 19:59:50 2003
 
     
========[ Invite a Friend - http://www.ganoksin.com/invite.htm  ]========


Hi All,
 
    I bet this has been debated before but I couldn't find it on line so
    what's the opinion out there? 

    I've owned 2 Durstons. One was a bargain because someone put a nail
    thrugh it and it had a goove, and the other was too small a 100mm and
    the rollers had mill marks on them. I have now saved up for a 120-130
    mm combo. I have seen a Cavallin locally for $750 and it seems to be
    the set up I want. All things being equal it has 65mm diameter
    rollers as compared to Durstons 60mm for the 120-130mm size-which is
    a plus especially compared to the 50mm dia. on the 100mm mills. The
    overall finish of the Durstons impresses me more as the Cavalin has
    some plasitic but we're talking dust sheild here so it's not
    important. 


    But have any of you with more experience put these mills through
    there paces and have strong opinions one way or another? This is
    basically a major purchase for me and I'd like to get it right
    finally. 


    Feel free to contact me directly at 

	notrix AT cox.net
	Thanks,
	Warren Allen
	Whatrix Designs
	http://www.whatrix.com

    ps I will finally be updating my site in the coming week as i have a
    table top studio set up and about 70 pices to photograph this
    weekend. W 


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project