>      Has anyone successfully glued gold foil onto paper, cut out the
>     design, and then dissolved the glue?  

    Something I have done to enable cutting out a design on gold foil
    that has worked very well is as follows: Get some white shelving
    paper from a hardware store and cut out a piece that is larger than
    the design. Draw the design onto the white paper, peel the adhesive
    back off part of the section of paper keeping the two parts still
    attached at one end. Slip the foil in under the design so that it is
    now sandwiched between the white paper and the adhesive backing. Cut
    out the design using very sharp manicure scissors and remove the top
    or white paper. Place the foil (upside down) onto the prepared
    silver on the hot plate, and the heat will coil up the adhesive
    backing and it can be picked off with a fine tweezers. (It can also
    be burned off) Replace the foil design in the desired position and
    proceed as usual to attach the gold to the back sheet. 

    I hope this is clear, but if you have any questions please contact
    me.  Joe Dule


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project