    Hi Shirl. My favorite adhering agent is Klyr Fyre which I get from
    Thompson enamel. It fires clear with no residue or problems. 
    Sometimes on flat surfaces  I use a very thin film of mineral oil on
    my copper to keep the grains  in place. i dab on just a wee drop,
    wipe it around with my finger, and then with a soft lint free cloth
    or piece of tisssue I wipe again to make sure that all I have is a
    film of oil. It works just fine, except on  sloped pieces, and on
    these i use either Klyr Fyre or a dilute mixture of gum Trag.   I
    have heard of Lotus Root powder, but have never used it. Also, some
    enamelists use hair jel as their adhering agent, but I would think
    it would have to be diluted as the stuff is thick and gummy. Perhaps
    some other enamelists will come up with some more solutions. Alma 



____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project