========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== When soldering bezels to a plate I heat from the side opposite the bezel. I set two fire bricks on a large solder pad. I leave a gap between the fire bricks slightly narrower than the plate. I set the edges of the plate on the fire bricks so that the bottom of the plate is exposed. I set the bricks slightly over the edge of a large solder pad. This allows me to direct the torch vertically against the plate. I mark the bezel side of the plate with a sharpie pen. When heating, the mark will start to disappear when medium solder temp is reached. At this point I play the flame on the bezel side of the plate. If the plate is very thin I move the bricks closer together but leave enough gap for the flame to hit the bottom of the plate. I use a large torch tip and heat the metal as rapidly as possible. Don't forget to coat all surfaces with an anti-firescale flux before each solder step. If you need a better description contact me directly and I will make up a sketch. Lee Epperson ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project