From: Steven Holden Date: Sat Oct 04 02:04:43 2003 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Hi, Sounds like a top heating problem to me...directing the heat directly at the bezel instead of heating the base up first, and I have to agree with another replier that fine silver bezel strip is much better for this work than sterling. I always try to get the whole piece off the surface of the soldering block somehow before starting to heat, as you can then get the flame under the base/bezel backplate of the piece before getting anywhere near to the bezel itself, and thus the bezel starts to heat up gently by conduction from the baseplate rather than getting the full frontal blast from the torch. I use either a third hand or rest the whole piece on top of a piece of scrap strip folded into a two thirds circle shape. Steve Holden in sunny Ibiza! www.platayflores.com ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project