From: Noel Yovovich
Date: Sat Oct 04 01:53:04 2003
 
     
========[ Invite a Friend - http://www.ganoksin.com/invite.htm  ]========


    Hi, Janet, As a former calligrapher, I can tell you that golf leaf,
    let alone gold foil, will not stick directly to paper. I don't know
    what "glair" is, but gesso is the usual. As an aside, for doing
    illuminated letters-- those gold ones with elaborate decoration
    around them in old manuscripts-- one depends on the fact that gold
    doesn't stick to paper. The part to be gilded is covered very
    carefully with gesso, even in tiny details. Then, after it is dry,
    the gold is applied and burnished down. A brush will wipe away
    everything that doesn't have gesso under it, so the gold is as
    detailed as one wishes. Multiple layers of gesso are used to create
    built-up letters. Believe it or not, coloring the gesso will change
    the way the gold looks, it is so thin, so the gesso is often red.
    The point about the layers of gesso is, you can probably control the
    texture by texturing the gesso with a brush when it is tacky (on
    maybe the third coat??) though I've never tried this. Good luck! 

--Noël



____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project