    Peter Rowe apologized for his "idiot" remark and I wanted to pass
    this on: The gentleman who advised me from Rio did clearly advise me
    to swish the ring in flux and that there would be no possibility of
    damage. There's no question that we both understood what I was going
    to do and how. He even said that if it hurt the stone that he would
    buy me a new one--and that is just what he has offered to do (and is
    doing, I think). I have never retipped a prong and the Rio person
    knew that. He was so nice and tried to be so helpful. I was sorry
    for both of us that it damaged the stone, because I could have so
    easily taken the stone out first but he assured me that that was not
    necessary. He said he had been doing this type thing for 30 years
    with no problem. The only thing that I can think of based on the
    posts that have been received is that maybe the created stone has a
    different makeup than some of the stones that this gentleman worked
    with--in other words, rubies used to be more safe to apply the torch
    near? Anyway, he was sweet, kind, and helpful--especially so. If it
    hadn't been for his help, I might not have learned so much from this
    experience. 

J. S. Ellington



____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project