>         ... ooops! I just took a look at my bottle of Batterns only to
>     discover that my Batterns is in fact Griffiths floride free flux. 


    Hi Bruce; That's what I switched to from Batterns.  I'll bet that's a
    contributor to the problem, since it seems the problem for me started
    at that time.  Have you noticed that the Griffiths seems to form a
    dirty looking foam as it melts?  I still suspect the silicon though. 
    Been a bit discouraging for my apprentice, as I've seen him having
    the same problem you describe in melting the area before the solder
    flows.  I've had to work to convince him it wasn't something he was
    doing wrong, since about half the time I take one that's gotten away
    from him and get it to work.  But then, I'm a bit slicker with a
    torch.  He'll be relieved to know I wasn't just trying to make
    excuses for him. 

David L. Huffman


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project