    John gave a very good tutorial on the water torches and I only have
    a couple of small comments.  Some of you may remember that our Gem
    and Mineral Society had obtained two old Krohn torches through a
    donation. I subsequently sent them to Krohn in NJ for refurbishing. 
    I must say that Alex, in the customer service department was very
    helpful and got them back to us quickly in great shape.  As these
    generators are no longer produced, he was able to provide some
    reconditioned fluxers and other items to keep the costs down. 

    One machine was traded for another piece of equipment but the other
    has been on our bench at the Society now for about a month.  It is
    great and one of our members uses it all the time for repair work and
    soldering bezels.  It is so clean, easy to use, and dependable I wish
    they were less expensive as I would love to have one in my own shop. 
    Perhaps as time goes on and more people use them, the price may come
    down a bit. 

    According to the Krohn manual, some heat control can be attained
    through the kind of flux used. The borax, methanol, and acetone mix
    provides a steady temperature around 4000 deg but by using only
    acetone the temp can go as high as 6000 deg.  Otherwise, there is no
    adjusting or guessing.  Just turn it on and work! 

    Cheers from Don at The Charles Belle Studio in SOFL where simple
    elegance IS fine jewelry! dcdietz AT comcast.net


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project