========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Normaly 24k is very resistant to wear. Historical studies have shown that 24k wears better than anything else, that lower carats (like 18, 14, 10K) abrade while 24k just gets mushed around. That means you can't keep a 24k surface intact but you can expect it to weigh well near what it started out at years later unlike most alloys. best Charles Charles Lewton-Brain/Brain Press Box 1624, Ste M, Calgary, Alberta, T2P 2L7, Canada Tel: 403-263-3955 Fax: 403-283-9053 Email: brainnet AT telus.net Our Collaborative information site to benefit the worlds' jewelers: http://ganoksin.com/ Over 500 pages of Charles' writing: http://tinyurl.com/k5v3 Book and Video descriptions:http://www.ganoksin.com/kosana/brain/brain.htm Gallery page at: http://www.ganoksin.com/brain/gallery.htm ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project