Hello All-

    This seems to be similar to the old Alexandruim (doped glass) that I
    was cutting 20 years ago, but all the material I acquired had a color
    change from lilac/rose de france to a light aquamarine blue. This
    material I was doped with Iridium. I recently bought a 2900-carat rod
    from a scientific supply company in California which has the same
    properties but the doping metal is Neodymium. The difference in this
    material is that it shows a triple colour-change: Lilac/rose de
    france in incandescent light, fine aqua in flourescent, and brilliant
    (like neon) green-blue in sodium-halide. I discovered the last color
    change when I wore a stone I had cut in a ring to the local Wal-Mart
    and someone commented on the pretty stone. I use the angles for beryl
    and get a pretty bright stone. 

    It is really too soft to place in a setting which will get banged
    up, but I'm considering making some unusual pieces with it: A
    "formal" eyepiece or monocle (it's laser material and completely
    flawless at low magnification) which would change color according to
    the lighting, circlets, neclaces with alternating aquamarine and
    lilac amethyst to mess with things visually, etc. Anyone else have
    ideas for this neat material? 

Cheers
Clyde Gilbert


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project