========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== All, I have cooked tigereye to a very nice red color in my barbeque. Beware tho, you can cook it too much and it will turn to a chalky red that is very brittle. I have never been able to obtain the three colors of red, blue, and gold by heat treating in one piece. All the pieces I have treated became totally red. My estimate is that a temperature of 450 -500 degrees fahrenheit is what is needed to change the color. Gerry Galarneau, in still hot Phoenix, Arizona. Cutting cabs from Crinoid Marble, Script Jasper, Picasso Marble, etc.... ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project