    First of all don't use a triangular file, even a #4 cut. You will be
    leaving a roughened surface and you just might have to polish the
    claws again. Have you ever thought of using a Flat graver #40 just
    for this operation? What you do is to sharpen the gravers cutting
    edge and place that edge just a little above the ">"  of the bearing
    cut. With a slow and deliberate cut in a careful downward motion,
    right to the base of claw itself. You will now observe two things...
    no filing has taken place, little need for polishing, and a very
    bright angled edge of the "bearing-cut". This will make a definite
    'finish' for the light to bounce off from the "pavilion" of the now
    set diamond. 

Gerry, the Cyber-Setter
gemz AT ican.net 
toll free cell phone 1-877-850-0003. 
http://www.gemzdiamondsetting.com


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project