    Lin-- You might want to check on the PMC Guild website for a lot of
    information (www.pmcguild.com).  Also, check out the metal clay
    groups on Yahoo.com--there are several ones you can sign up for. 

    As to your specific question regarding the hot pot, that was
    mentioned just the other day on the "metal clay" group on Yahoo.  To
    quickly summarize:  The hot pot is not hot enough to include enamels
    with your PMC.  It is not good for PMC regular or PMC+ (or the Art
    Clay equivalent)--just the PMC-3.  You can add some synthetic
    gemstones  and sterling silver findings, but not glass due to
    temperature sensitivities.  The ceramic fiber hot pots were
    considered to be more durable than the ceramic hot pots--ceramic hot
    pots had a tendency to break more easily and crack. 

    I would think that if you could get some sort of temperature gauge
    on your mini-kiln then it would be fine for PMC.  Anything will do
    as long as it holds the correct temperature for the right amount of
    time.  

Have a blast with the stuff!
Laura


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project