    I expected more replies to the question of setting the heart-shaped
    "briolette" than there have been. So, I guess I'll jump in. 

    If I understand correctly, you want a bezel that runs around the
    edge, leaving both sides exposed. You cannot expect to solder around
    the stone. With a typical cab, you would make a bezel as
    usual--strip of fitted bezel wire on a backing, then cut out most of
    the backing. You would leave a narrow edge to hold the stone in, and
    close the bezel over the top. 

    In this case, the "back" is the same as the front. I think I would
    try doing a fitted strip od bezel wire, as usual, and solder it to a
    thin backing of fine silver. Then I would cut out all but the edge
    of the backing, and shape the backing to the stone as one would a
    bezel. Then close the bezel on the other side. Fine silver is *much*
    easier to form than sterling, so it shouldn't be too hard. If you
    file and polish nicely, it should come out very pretty. 

    If this isn't clear enough, let me know and I'll try to draw a
    better word picture. HTH!      

--Noel


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project