    Ok, here's my 2 cents worth.  I have a Bransonic 1210 heated unit
    now, but I once had a 2 cup capacity ultrasonic that was my favorite
    by far.  I have to change the solution every day anyways.  I learned
    from my elders (lol) to use 9 parts hot water and 1/2 part each of
    clear ammonia and Mr. Clean ( the original tennis ball green color).
     This works better than any commercial solution I have tried.  My
    tool of choice for putting jewelry in the cleaner is a plastic juice
    strainer.  It won't scratch the jewelry, and if you're putting
    earrings in, the posts will go through the mesh so the earrings
    won't touch.  I also have one of those racks for rings and pendants,
    but it's my second choice). If the rouge won't come out It's usually
    behind a stone and I use a small dental tool to unlodge it or an old
    toothbrush (which sometimes scratches). 

    P.S.  I was also taught to strain the used solution through a paper
    towel placed in the strainer.  This goes in the recycling bucket. 

wendy newman
www.goldgraphix.com



____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project