========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== I took everyones advice and cast with a shorter and larger sprue with a resivior and I switched to silver as I don't know for sure the melting point of this bronze. It cast really well so I think I have the issue fixed. I am doing a 10 kt gold cast tonight I hope to have good results. I got a pyrometer also and found that pretty much every machine I had was un calibrated to some degree one was off by 100 degrees which prolly doesn't make things better. It's a digital pyrometer for 70 dollars I'll not spam the link cause I dunno the rules about that if you e-mail me i'll send it to you. Thanks for all the help. ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project