    I read this thread and it covered almost everything I could think of
    and add some. I never would have thought of lowering the temp of the
    wax. I have lowered pressure and that has worked. Thanks Orchid for
    new insights. Here are a couple of things that no one else mentioned
    that I thought I might add to this very productive thread. 1. Use
    corn starch instead of talc. Talcum powder is a mineral and cannot
    be absorbed by the body. It builds up in the lungs just like coal
    dust. Not good. Corn starch can be absorbed as it is organic. It
    works just as well as talc. 2. I sometimes use a #62 drill bit to
    vent a specific area that is giving real trouble. It leaves a little
    nipple that is very easy to clean off . I find that knife vents can
    sometimes lead to mold distortion if cut too deep. The drill vents
    are less intrusive to the rest of the pattern and much more spot
    specific, although they do need occasional cleaning.


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project