    Just exactly what is Bali silver?  I just came back from this
    weekend's International Gem Show (Marlboro MA), and again, I'm
    confused about the silver beads and findings currently on offer.  

    Sterling silver ("bright" or "white") looks like pickled polished
    sterling.  But a lot of this "Bali" stuff is much darker even though
    highly polished, and if you look at it closely, the dark stuff in
    the crevices is NOT polishing compound or patination - it chips off
    like some kind of lacquer.  And all of a sudden this stuff is .30 -
    .35/gram, rather than the .60 - .80 it was recently. WHAT is this? 
    Is it a different alloy?  Non-silver?  Plated?  Does anybody out
    there know what I mean??  

    Help, please - I'm going back tomorrow and I need findings! 

    Tas <-- grumpy, because she used to know EVERYthing 



____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project