    Hi, On occasion we have customers who send us castings that have
    parts soldered on with lowmelt lead solder. This type of solder will
    usually melt in a vulcanizer ( not good) so what we have done when
    we see this potential problem is this... We put it in our smallest
    pickle pot with sparex /water and heat it to about 150  oF and leave
    it in the pickle until the finding falls off and the solder
    completely disintegrates off of the silver or gold item. Afterwards ,
    there is usually a very tiny grey area that can be wiped off with
    fine emery paper.   If the pickle is still good, we will keep it in
    a glass jar for other similar situations. 

    Hope this is helpful. 

    Daniel Grandi,  www.racecarjewelry.com We do casting finishing and a
    whole lot more for designers, stores and people in the trade. Contact
    us at   sales AT racecarjewelry.com Or call 401-461-7803 



____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project