From: Katherine Palochak Date: Fri Jul 11 03:19:35 2003 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== This works for me, and I've been doing a lot of snake chains this past year in various terminations. Use ochre mixed with alcohol. Apply a thin 1/8" strip below the area that needs to be soldered. Make sure you hold the chain so gravity doesn't cause it to flow where you want to solder before the alcohol evaporates. Heat it up gently until the ochre turns a dark red-brown, and not to much heat so that the chain oxidizes. Apply just a bit of flux (I use a short dowel rod to roll the flux on without overdoing it). Pick up a small ball of solder on your pick or tweezers. Touch it to where you need to solder when it's up to solder heat. After you're done soldering, put it through a pickle, then if you happen to be lucky enough to have an ultrasonic, it will take care of the flux and ochre. If you don't have an ultrasonic, boil it with water and a little dish soap. Kind of involved, but it works well and you have a professional looking end, without any fused areas. ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project