    Dear CameoArtist, Way back when I first started cutting stones I
    learned from this old hippy guy who told me that the original cameos
    were done from black and white striped onyx.  The stone was shaped
    and then the woman's head was carved as a bas-relief leaving the
    black part of the stone as a background.  I can't verify this but I
    have seen some very old cameos and they did indeed look like they had
    been carved from a single two color stone.  I think onyx (a form of
    cryptocrystalline quartz) might be a little harder to cut but much
    more forgiving than seashell, and less hazardous to your health. 
    There are deposits of this type of onyx out here in Arizona, and you
    can sometimes find the rough sold in massive form at the Quartzite
    gem show in late January just before the big Tucson show. 

    Another thought is using opal as your cameo material. 

    As a disabled person I think your training is a great thing.  After
    I became disabled and could no longer walk or sit up all day
    programming computers I had something to fall back on that gives me
    something to do and maybe I might even make a little money at it one
    of these days. God Bless Rick Carew AZopals  r_carew AT cox.net


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project