Hello Charles-

    According to Lange's Handbook of Chemistry, 12th Edition, page 4-107
    and Handbook of Chemistry and Physics, 82nd Edition, p. 4-83, silver
    permanganate (CAS Reg. No. 7783-98-4) is violet to dark violet
    monoclinic crystals, solubility in water of 0.9 grams per 100 grams
    of water and decomposing in 95 percent ethanol.  It doesn't look
    like it would be inert enough to be useful on jewelry.  Since you
    are a DDS, I know you have had sufficient chemistry to be aware of
    the explosive hazards of permanganates.  I blew up a burette right
    next to the Professor in a quantitative analytical lab one time.  I
    was trying to clean the thing with a conc. sulfuric acid/potassium
    permanganate solution when the classical sodium dichromate/ sulfuric
    acid mixture was not effective.  The thing went off with a heck of a
    loud bang and totally shattered the burette.  Fortunately, no one
    was hurt or sprayed with acid.  I was holding the burette down in a
    deep soapstone sink. 

Captain Blood
"Marlinespike Seamanship in Precious Metals"
mariner AT tgtel.com



____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project