    Hi all.  I really have been pleased using acid (pH minus) instead of
    Sparex. Thanks Orchid and John Burgess! 

    Lately though, as I've been using Prip's flux more often I have
    discovered a warm alum solution is superior for removing that
    tenacious post-Prip's glaze.  Thanks again to Orchid and friends! 

    My question concerns potential problems when using alum. 

    -Is there any difference in action or safety among the various
    "alum" compounds available? 

    -Would prolonged immersion in alum solution affect the metals or the
    solder joint?   

    -Are there conditions that would produce plating of dissolved metal
    ions?  

    -Are there metals or stones which should not be placed in alum
    solution? 

    -Any situations where acid might be preferred over alum solution? 

    In searching for a more reasonably-priced source than buying alum in
    the spice aisle, I have found aluminum sulfate, as a mordant in
    fabric dyeing, available at $2.75 / lb. and $10.95 / 5 lb from this
    website:  http://www.dharmatrading.com/html/eng/3334-AA.shtml Thanks
    in advance for enlightenment. :-) Pam Chott Song of the Phoenix


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Blogs
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2009, The Ganoksin Project