I have found that a brass brush in a flex shaft does a great job of
cleaning files. Use a very light touch and move the wheel at low
speed across the file in the direction of the riffles. Cheers from
Don at The Charles Belle Studio in SOFL where simple elegance IS fine
jewelry! dcdietz AT attbi.com