    I bought some "Amethyst" - large, gorgeous, faceted drops, great
    price, at the recent wholesale show in Greensboro, NC.  I was
    doubtful at the time that what I had was actually Amethyst given the
    apparent perfection and low price, and have had others look at them
    since who agree with me.  I suspect what I have are some really
    gorgeous very large glass drops - which is really what I figured I
    was buying ;) no matter what they called them. 

    When I loupe them I don't see any bubbles though - should I if they
    are glass? 

    Also, it turns out they are color change - whatever they are! 
    Switch light sources, and they switch color.  Very pretty!  I was
    selling them individually (the ones I thought I didn't want) at a
    recent SFMS workshop, and had a "run" on them once folks found out
    they color changed - like me they didn't care about the actual
    material, just that they are really nice large drops. 

    Anyone else run across these?  Suggestions on telling what they
    really are with a loupe? 

Thanks!
Beth in SC


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project