Hi Dede,

    I have a theory about why Tiffany Sterling does not seem to tarnish
    as quickly as other sterling jewelry. 

    I think the main reason is that people tend to keep their Tiffany
    jewelry in the Tiffany box and in the blue felt pouch. It could be
    that the box is made from low sulphur paper or perhaps the felt is
    treated in someway (perhaps like Pacific cloth?). Even if the box or
    the felt are not treated, just keeping the sterling jewelry in a box
    and in felt would lower the amount of air circulation and humidity
    that causes unprotected pieces to tarnish faster.  It also could be
    that Tiffany may treat the piece with something like 3m's Tarnishield
    that will help prevent tarnishing for a while. 

    People are proud to own a piece made by Tiffany and the box and
    pouch are rarely discarded. They are kept and used. Other sterling
    jewelry does not have the "cachet" and tends to be kept unprotected. 

    I have a pair of Tiffany cufflinks that I've kept unprotected on top
    of my dresser (in a tray along with my loose change!) for a month and
    they have tarnished as badly as the "off brand" sterling chains I
    keep in the same tray. 

    Dan T. 

    PS. I've discovered that you should never wash a poodle with Suave
    Dandruff control shampoo... He smells HORRIBLE. 



____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project