From: M'lou Brubaker Date: Sun Apr 27 23:20:11 2003 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Rick, I got some yellow tarnish, also, on silver that I had just finished and washed and then put immediately into plastic bags. Since most of my work has been treated with an oxydizer, I felt that maybe I needed to more completely dry the pieces before zipping them up in a bag. I think that the slightly damp corners and recesses which had been oxydized might be, as they dried, off-gassing some residual oxydizer into the tiny air space of the plastic bag, and affecting the whole piece slightly. I now air dry all jewelry for a few hours before zipping it up in a bag, and I have not been seeing the yellow discoloration any more. HTH! -- M'lou Brubaker mlou AT uslink.net ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project