| Re: [Orchid] Backing Moonstones | ||
|
[Thread Prev]
[Message Prev]
[Date Index]
[Thread Index]
[Message Next]
[Thread Next]
From: Kaytzbdz Date: Sat Apr 26 22:24:05 2003 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Dear Sandra, Another Orchidian (thanks, Donna) shared with me that to raise cabbed stones to a desired level, use the plastic (comes in variety of thicknesses) that model train people use to make the little windows in the train cars. You can cut to size, stack, and set. And it doesn't deteriorate. Use this instead of sawdust to back the stones for example. I have used it that way, and also have used permanent paint pens found at art stores to color the plastic shape that will back a stone or bead. The resulting color under the translucent stone or glass bead (cut and cabbed) can be very subtle by mixing, stacking, etc. or very obvious. Turn the painted surface upside down for a very subtle difference, but of course, the color effect would be reversed. Find the plastic sheets (fairly more expensive than you think they might be) at model train shops. The clear plastic does come in some colors, as I remember, aqua and yellow, and of course clear. Kay Taylor ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project