From: DaniP Date: Fri Apr 25 23:15:41 2003 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Hi everyone. In my ongoing quest for the kind of resist I can use to create many detailed designs quickly, one of my fellow jewelers suggested using wax. I figured I would tap into this community's knowledge before I make myself crazy. Does anyone use wax as a resist when working with silver doing etching in ferric nitrate? What I am finding is that the nitrate eats all of my paint pens and causes serious pitting. I am tired of ruining perfectly good pieces of silver, and while I wait for my nail polish pen to arrive for my next test, I thought I should ask if anyone uses wax or any other unconventional resist to work their deigns in silver. Thanks in advance for your help! -Dani ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project