    To reduce a stones exposure to excessive heat when soldering try
    this. Get a pet food can or tuna fish can and a lid plastic which
    will tightly fit it . Fill the lid nearly to the top with clean fine
    sand. Wash the sand if needed. Add enough water to make it very wet
    yet moldable. Then squish the sand into a M shape and place the ring
    sticking out of it Deeply bury the gemstone and leave only the shank
    or offending portion exposed. When You add boric acid, paint on and
    burn off the alcohol several times. Use enough to make a pasty
    covering on the sand it is cheap. This protects the stone from heat
    and the ring from oxidation . When You solder , place the solder on
    the top and heat from below up . A smith little torch with a #  6 or
    7 tip will produce a large QUICK heat . Place the lid on the can until
    it is next needed. 

ROBB



____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project