From: Renate Sommer
Date: Fri Apr 04 20:33:00 2003
 
     
========[ Invite a Friend - http://www.ganoksin.com/invite.htm  ]========


>      I am using a paint pen, and the pen is flaking into the ferric
>     nitrate and the etchant is pitting parts of my silver and etching
>     through parts of my design. 

    Dani, I have no experience with a paint pen but have good success
    using Bituminous Paint as a resist. Paint the whole surface and
    scratch out the design or paint the design on .... either works
    quite well. You can get Bituminous Paint in hardware stores in
    Australia, used for painting on pruned tree branches (among other
    things I think). 

    I use a cocky feather to brush away the bubbles as they form. Hope
    this is of use. 

    Renate, from Adelaide, Australia where the cockys are wreaking havoc
    on the ripening walnuts.


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2007, The Ganoksin Project