From: Karen Christians Date: Fri Apr 04 20:31:27 2003 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== The BEST resist pen I have found so far is the Staedler red permanent ink pen. I got this tip from Sandra Goss who uses it in her etching. Doesn't matter if it is ferric nitrate on silver, or ferric chloride with copper or brass. The photocopy resist works very well, if you keep the metal clean, and apply a 3 alcohol to 1 water mix. Denatured is the best. If your toner runs, alter the proportion until it stops. Keep the metal a little wet when you apply your transparency film and squeegee out the excess. This sucks the film right onto the metal and you get much better results. If you get little "blooms" or clear spots, touch this up with your pen. Good luck! -k ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2007, The Ganoksin
Project