From: JETT Research Date: Fri Apr 04 20:31:07 2003 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== > would you give us more information on an ion exchange > column please,and how to make ,or where to purchase? thank you One source of the columns and pumping system hardware is Harrington Plastics. They do not supply the resins, just the hardware and you can easily find them on the web. There are several companies that supply ion exchange resins but do not supply the hardware. There are even a couple of refining companies that supply the resin "free" if you are refining with their company. I don't usually avail myself of that because I can assure you that nothing is really free. A company named Rohm and Haas make resins for many different industries including precious metals recovery. There is also a company named Serfilco (http://www.service-filtration.com/Ion-Exchange-Systems.html), that seems to be reasonable. They also make and sell the tank and pump hardware as well as the resins. If they sell the hardware and the resins, I tend to think that they are more familiar and will provide better support. I have been wrong on this count many times before. Best Regards, J. Tyler Teague JETT Research ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project