>        All the other stuff written about alloying, while informative
>     from the point of view of making white gold, is moot because that
>     isn't what happened. 

    On the contrary Daniel, It may not be that simple. The piece may have
    been molded and cast. This may have been explained to the customer.
    They may have had no idea what the jeweler was talking about all
    they knew was that their piece was now white. If she believed that
    someone could magically change the molecular structure of an alloy
    she probably couldn't grasp molding and casting. 

    Here in Colorado gold aspen leaves are popular. I have had customers
    bring in leaves they picked up while hiking and asked me to dip them
    in gold. Yes, they think you can just dip them in liquid gold. I
    tell these people about the melting temperature of gold and how
    leaves burn and they look at me and say "well, a guy in Telluride
    does it" .... 

    I understand that there are thieves and hacks in this business but I
    also know that there are many, many, many customers who are clueless
    when it come to jewelry concepts and technology. I hope that it was
    the latter in this case. 

John Sholl
Littleton, Colorado


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2007, The Ganoksin Project