>     You use the  stuff that ends up in the middle tray to get the
>     clear transparents. 

    I am using a lot of transparents and it is not enough to sift them,
    you need to wash it. Put the sufted enamel in a glas or a container,
    depending on how much you need to wash. Put water on it, stirr with a
    glass or plastic spoon, leave for some seconds so most of the enamel
    sinks to the bottom. Pour the water off, not too fast but watch the
    enamel on the bottom carefully: don't throw that away. Repeat as many
    times as you need to get clean water on top. (throw the water in a
    container to collect the enamel and don't wash it away in the sink).
    In the place were I live (Maastricht) the water is very hard and will
    leave a cloudy residu in the enamel, so I end up with washing twice
    with destilled water, the kind you can use to fill the steam ironing
    iron with. Hope this helps, just done a lot of transparents and they
    were all perfectly clear, also the Thompsons can become clear! Needs
    to be fired at the right temperature too, and be careful no dust can
    fall in while it is drying. I hate it, but you must always work in a
    clear worspace. (There is no place in my house as clean as my
    enameling space while I am enameling). 

Hope this helps, good luck! Marleen.
Marleen B.Berg
Aventijnhof 11
6215 ES Maastricht
Nederland
website: http://www.mbberg.com/


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2007, The Ganoksin Project