| Re: [Orchid] Yellow cloudiness in enamels | ||
|
[Thread Prev]
[Message Prev]
[Date Index]
[Thread Index]
[Message Next]
[Thread Next]
From: Karen Seymour-Ells Date: Mon Mar 31 22:32:05 2003 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Hi, I will readily admit that I don't do much firing of transparent enamels on silver, so I'm not the expert you were looking for. You don't seem to be getting a lot of response on this though so I would like to state two common problems it could be. 1) As someone else mentioned, to get really clear enamels you need to remove the fines, or the powdery enamels that exist after grinding. You need a little bit but not as much as is normal. Tom Ellis did this by using 3 layers of sifting trays. 150 mesh on top, 325 mesh in the middle and a catch pan on the bottom. You use the stuff that ends up in the middle tray to get the clear transparents. He said to discard the fines, but most of us use them as counter enamel instead. 2) Many enamelists complain that they can't get a truly clear enamel on silver from Thompsons. I agree that you should try Tom Ellis at Thompsons and ask, but don't limit yourself to just that. You may also want to call Coral Shaffer at 800-596-3257 or 206-525-9271, she sells imported enamels that some of my friends have much better luck with, of course, these are not lead-free as Thompsons are. Karen ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project