From: Dave Arens Date: Sun Mar 30 22:54:51 2003 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Hi Larry, If you want to melt jump rings to make granules here's a way to figure the size of jump ring to use. 1. Calculate the volume of the granule. 4/3 times pi times the radius of the granule cubed. e.g.. 3 mm granule, 3/2= 1.5, 1.5 x 1.5 x 1.5 = 3.375, 3.375 x pi = 10.6, 4/3 x 10.6 = 14.14 cubic mm. 2. Select the wire to be used to make the jump rings. e.g.. 16 ga (1.29 mm). 3. Find the length of 16 ga wire that'll have a volume of 14.14 cubic mm. e.g.. pi x radius squared x length = volume. 1.29/2 = .645, .645 x .645 = .416, .416 x pi =1.307mm. 14.14 /1.307 = 10.82 mm. A length of 16 ga wire 10 82 mm long will have a volume of 14.14 mm. 4. Find the size jump ring that has a circumference of 10.82 mm. e.g.. 10.82/pi = 3.44 mm. A 16 ga jump ring 3.44 mm in diameter will have a length of 10.82 mm & a volume of 14.14 cubic mm. If you get real technical about these calculations the volume will be off a little, but I doubt anyone will notice unless you're making granules for NASA. The methodology can be used for any size granule & any size wire. Dave ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project