    Sorry, I didn't mean to be vague in my first message.  :)  I'm using
    lead-free Thompson enamels that are fairly new, I bought their
    sample set just a few months ago.  I have been enamelling on fine
    silver, and have done tests using their clear for silver, golden
    clear, medium clear, and hard clear.  I have also tried some tests
    on copper, both with and without silver cloisonne wires.  I'm
    currently sifting the enamels through a 100 screen, then washing
    with distilled water.  I've been applying them with Klyr-fire
    diluted with distilled water.  The only reason I mentioned the kiln
    is because it is also new.  Up until now I have been enamelling at
    the local community college, in a very old well used kiln, and had
    never noticed this particular problem.  The one I recently bought is
    the same model, but I had noticed a lot of powder coming from the
    walls when I open and close it, so this weekend I painted the walls
    and inside of the door with fiber hardener.  I've only tested it
    once since then, but had the same results.  The only thing different
    between this kiln and the one at the college (other than the age) is
    that this one has a porcelain tray that sits in the bottom.  I think
    its actually a burnout tray, but I left it in there to protect the
    bottom of the kiln. Thanks again, Susan


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project