========[ Invite a Friend - http://www.ganoksin.com/invite.htm  ]========


    Teresa, I get silver paste solder in syringes from Hagstoz in Philly,
    but have also gotten them from Rio. 

    Hagstoz' phone is 800-922-1006. 

    Rio's paste solder seems to no longer be sold in syringe form, but
    is in jars. 

    However, in any case you could easily get appropriate syringes and
    fill "as needed" from the jar -- would probably keep a little better,
    too.  To get small syringes (without needles) cheaply (or for free),
    check with your local veterinarian.  They use them all the time for
    vaccines and other relatively clean uses, and take the needles off
    for medical waste discards. The syringes themselves are thrown away. 
    If you don't mind cleaning them (take out the stopper and wash
    thoroughly in a bath of hot water and soap, then lay in the sun to
    dry), you'll have a wonderful source in just the right size.  If you
    DO mind cleaning them, ask your vet if s/he will order some on your
    behalf (they are ordered without needles) if you pay for them. Take a
    look, but the 3ml size is probably ideal for most jewelry uses. 

    As long as the syringes are purchased without needles, they are
    perfectly legal to have without a prescription.  With the needles,
    you need a prescription.  (At least here in the U.S.) 

Good luck!
Karen Goeller
kgoeller AT nolimitations.com
www.nolimitations.com


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project