From: Donna Wilson Date: Wed Mar 26 23:06:25 2003 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== > I was recently told that I should not use the same kiln for > enameling as I do for burnout. I'd always heard the same thing about burnout kilns and enameling. In the summer I usually teach an enameling class. I bring in two of my small kilns and use the jewelry class burnout kiln as a third kiln. I've been doing this for 4 years. I note no differences in the appearance of the enamels fired in the burnout kiln as compared to my "enamels only" kilns. Everyone is using the same set of Thompson enamels and often the same colors. I always make sure that the burnout kiln is vacuumed out and very clean inside. Donna in VA ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project