>      This raises an interesting question. Can silver and gold be cast
>     in a respectful way to nature?  Is traditional casting process
>     respectful to nature? What about standard polishing? 

    Actually, The answer is yes... There are ways to do almost any job in
    an ecological manner. Casting can be done in this way, but many
    manufacturers don't. Many companies use "bombing" , a cyanide based
    method to remove firescale after casting... and as a result, some
    companies dump their cyanides down the drain or use improper
    /incorrect methods to destroy the cyanide before dumping. Silver ,
    left over from the bombing ....if it gets into the sewage system,
    will cause major problems in many sewage plants. 

    Disposal methods for Casting investments can also be done in a
    correct manner a ccording to your state laws... many do not follow
    this, or are not aware of the laws. 

    Many companies do not steam dewax, so the majority of their wax goes
    up the chute. 

    Your lucky DeDe, You can tell your customer that your castings are
    done as ecologically as possible. We don't use any dangerous
    chemicals of anykind ... recover our wax and reuse it for different
    purposes, dispose of our investment according to state disposal laws
    we are in  the process of finding other uses for used investment and
    90 % of the water we use in all other processes are reused through
    various methods until the final amount evaporates. 

    So, Yes,It can be done....... Daniel Grandi    Racecar Jewelry Co.
    Inc.  We do casting, finishing , molds, models, enamel, soldering,
    assembly for designers ,students, jewelers and people in the trade . 
    contact: sales AT racecarjewelry.com


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project